Electrical Contact Tips
Product Features:
Argentum cadmium oxydatum electricum contactum materiae late adhibetur, punctum contactuum humile liquescens in contactibus sublimationis facere potest refrigerationem contactus superficiei et simul exstinguere effectum, ne contactum incendat.
AgSnO2, AgSnO2In2O3 contactu commoda altae duritiei, resistentiae fusioni glutino et resistentiae ad ustionem elc.
Materia optima est materia praesidii environmental reponere AgCdO.
Applicatio: |
Contactores, murorum ambitus, thermostatorum, virgas intelligentium, etc |
Materia: |
AgZnO , AgSnO2, AgCu , AgCuO , AgCdO , AgNi , AgSnO2In2O3, AgSnO2/Cu , AgCdO/Cu etc. |
matriral | Wt% | G/cm3 | μΩ.cm | Mpa | % | HV:KGF/MM2 |
AgCdO10 | 90 | ≥10.1 | ≤2.10 | ≥260 | ≥15 | ≥50 |
AgCdO10 | 88 | ≥10.0 | ≤2.2 | ≥260 | ≥12 | ≥60 |
AgCdO10 | 85 | ≥9.85 | ≤2.3 | ≥260 | ≥10 | ≥65 |
AgCdO10 | 83 | ≥9.8 | ≤2.4 | ≥260 | ≥8 | ≥65 |
AgSnO2(8) | 92 | ≥9.9 | ≤2.3 | ≥250 | ≥17 | ≥70 |
AgSnO2(10) | 90 | ≥9.8 | ≤2.3 | ≥250 | ≥15 | ≥75 |
AgSnO2(12) | 88 | ≥9.7 | ≤2.4 | ≥260 | ≥12 | ≥80 |
AgSnO2(5)In2O3(3) | 92 | ≥9.9 | ≤2.3 | ≥250 | ≥17 | ≥75 |
AgSnO2(5)In2O3(4) | 90 | ≥9.8 | ≤2.4 | ≥250 | ≥17 | ≥80 |
AgSnO2(5)In2O3(4) | 88 | ≥9.7 | ≤2.5 | ≥260 | ≥12 | ≥85 |
Processus principalis:
excoquunt
extrusionem
calidum volubilem
frigus volubilem
Inspectis sarcina
Superficiem treatment
Internum oxidized
terunt
Pelagus Application